DISCLAIMER: The Graph Chatbot is not programmed to provide explicit or categorical answers to your questions. Rather, it transforms your questions into API requests that are distributed across the various IT services officially administered by EPFL. Its purpose is solely to collect and recommend relevant references to content that you can explore to help you answer your questions.
(La0.6Sr0.4)0.95FeO3-δ/ Sm0.2Ce0.8O2 (70:30 w/w) and (La0.6Sr0.4)0.995Co0.2Fe 0.8O3-δ/Gd0.1Ce0.9O 2 (50:50 w/w) cathodes screen printed on anode-supported cells were tested for 500 h under different conditions by using a Taguchi matrix that combined cathode processing parameters (cathode material, thickness, sintering temperature) and operation conditions (temperature, current density, air flux, air humidification and chromium presence). Individual effect of each control factor on cell performance degradation was evaluated: chromium poisoning, air humidity and temperature were classified, in such order, as the most influencing parameters for cathode and cell degradation. Unexpected high degradation rates were estimated at 750°C. Limited influence of the type of cathode on long-term behavior of cells was found; LSF/SDC cathodes exhibited, however, higher long-term stability.
Sophia Haussener, Venu Gopal Agarwal
Sophia Haussener, Saurabh Yuvraj Tembhurne, Alexandre Dominique M. Cattry, Matthieu Jonin, Mahendra Patel
Sophia Haussener, Evan Fair Johnson