DISCLAIMER: The Graph Chatbot is not programmed to provide explicit or categorical answers to your questions. Rather, it transforms your questions into API requests that are distributed across the various IT services officially administered by EPFL. Its purpose is solely to collect and recommend relevant references to content that you can explore to help you answer your questions.
Charge transition levels of dangling bonds in III-V semiconductors (AlAs, GaAs, and InAs) are determined via hybrid density-functional calculations. In GaAs, the Ga and As levels are found at 0.28 eV below the conduction band and at 0.16 eV above the valence band, respectively, in good correspondence with measured levels. These defect levels line up across the present semiconductor series for a band alignment based on experimental offsets. For In0.53Ga0.47As, both the In and Ga levels are inferred to resonate with the conduction band while the As level remains in the gap at 0.1 eV from the valence band. (C) 2010 American Institute of Physics. [doi:10.1063/1.3515422]
Giulia Tagliabue, Alan Richard Bowman, Fateme Kiani Shahvandi, Theodoros Tsoulos
Giulia Tagliabue, Alan Richard Bowman, Fateme Kiani Shahvandi, Theodoros Tsoulos