DISCLAIMER: The Graph Chatbot is not programmed to provide explicit or categorical answers to your questions. Rather, it transforms your questions into API requests that are distributed across the various IT services officially administered by EPFL. Its purpose is solely to collect and recommend relevant references to content that you can explore to help you answer your questions.
Tungsten-iron alloy was produced by electrodeposition. The electrodeposited alloy (15 at.% W) possesses a two-phase composite microstructure, containing a nanocrystalline phase of distorted BCC structure with a grain size between 50 to 150 nm and an amorphous phase as the matrix. TEM in-situ annealing revealed that this composite structure was stable up to 650 degrees C. When tungsten content was doubled, the deposited alloy became amorphous.